Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low to high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm
0.00050 - 0.0020 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.6 MPa
11400 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 7.72 GPa
1120 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 123 MPa
17800 psi
ASTM D790
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 6.35 mm
216 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C

@Thickness 6.35 mm
207 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm - 1e+05
1000 ohm-cm - 1e+05
ASTM D257
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ASTM D257
Static Decay 0.0020 sec
0.0020 sec
(Mil-B-81705C), 12% RH, 5000 kV to 50 kV
Processing Properties Metric English Comments
Melt Temperature 227 - 238 °C
441 - 460 °F
Descriptive Properties Value Comments
Features Antistatic
Conductive
Electrically Conductive
Statically Conductive
Filler / Reinforcement Carbon Fiber Reinforcement, 13% Filler by Weight
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Aerospace Applications
Automotive Electronics
Business Equipment
Computer Components
Connectors
Electrical Housing
Electrical/Electronic Applications
Housings
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved