Mechanical Properties Metric English Comments
Flexural Strength 123 MPa
17800 psi
ASTM D790
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free..
Flexural Strength 123 MPa
17800 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC
LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated.
Flexural Strength 123 MPa
17800 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC
LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing.
Flexural Strength 123 MPa
17800 psi
ISO 178
Nilit FRIANYL A63 HS-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced
Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Strength 123 MPa
17800 psi
ASTM D790
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66
Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon.
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East)
LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
Flexural Strength 123 MPa
17800 psi
ISO 178
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Strength 123 MPa
17800 psi
ASTM D790
Techmer ES HiFill® ABS GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Flexural Strength 123 MPa
17800 psi
ASTM D790
Techmer ES HiFill® ABS GF15 BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Strength 123 MPa
17800 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS
LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare.
Flexural Strength 123 MPa
17800 psi
ISO 178
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66
LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 123 MPa
17800 psi
at rupture; ASTM D790
Sumitomo Bakelite North America E 9405H-1 Glass Filled Electrical Encapsulation Grade Epoxy
E-9504H-1 is glass fiber filled epoxy molding compound designed for encapsulation of delicate electrical components as well as large coils. Excellent thermal shock, moldability, and retention of ele..
Flexural Strength 123 MPa
17800 psi
ASTM D790
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc.
Flexural Strength 123 MPa
17800 psi
ASTM D790
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Flexural Strength 123 MPa
17800 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS
LNP* THERMOCOMP* AF004 is a compound based on ABS resin containing 20% Glass Fiber.
Flexural Strength 123 MPa
17800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MX00709 PP
LNP* THERMOCOMP* MX00709 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this grade are: Heat Stabilized, UV Stabilized.
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled
SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers
Flexural Strength 123 MPa
17800 psi
ASTM D790
Plenco 6015 Phenolic, Briquette, Injection Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
Flexural Strength 123 MPa
17800 psi
ISO 178
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester
BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o..
Flexural Strength 123 MPa
17800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC
LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Flexural Strength 123 MPa

@Temperature 150 °C
17800 psi

@Temperature 302 °F
3.5% Strain; ISO 178
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Flexural Strength 123 MPa
17800 psi
ASTM D790
Techmer ES HiFill® ABS GF15 A1 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.