Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ISO 294-4 |
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber High stiffnessInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Time 86400 sec |
0.0010 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI (Asia Pacific) LNP* Thermocomp* ECF62 is a compound based on Polyetherimide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Time 86400 sec |
0.0010 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |