Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Nymax® 600 Series of mineral-reinforced nylon 6 compounds have been specifically developed to provide an excellent balance of physical property performance and durability, with improved surface appearance. These materials have been formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Water Absorption 0.90 %

@Thickness 3.18 mm
0.90 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 89.6 MPa
13000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Yield 14 %
14 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 141 MPa
20500 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 200 °C

@Thickness 3.18 mm
392 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 3.18 mm
212 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Filler / Reinforcement Mineral Filler
Unspecified FillerReinfor., 40% Filler by Weight
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved