Material Notes:
The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as Molded SAP Code: EM0C904174*Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 1.0 %

@Thickness 3.18 mm
1.0 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ISO 294-4
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
Type I, 5.1 mm/min; ASTM D638
90.0 MPa
13100 psi
ISO 527-2
Elongation at Break 6.0 %
6.0 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 3.28 GPa
476 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 141 °C

@Thickness 3.18 mm
286 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Additive Impact Modifier
Appearance Black
Features General Purpose
Impact Modified
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Copyright © lookpolymers.com All Rights Reserved