Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 3.28 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Multibase Multi-Pro® 4006 TH Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Multibase Multi-Pro® 4012 TH Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase
Flexural Modulus 3.28 GPa
476 ksi
ASTM D790
PolyOne Nymax™ GF 1010 14 Black 13 Polyamide 6 (Nylon 6)
The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of ..
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Omni Plastics OmniTuff™ CPP TF30 Copolymer Polypropylene Talc Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Oxford Polymers 901-BK Polycarbonate/Polyetherimide Alloy
Polycarbonate/Polyetherimide AlloyInformation provided by Oxford Polymers.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Oxford Polymers OPX782 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads
Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers.
Flexural Modulus 3.28 GPa
476 ksi
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data)
Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat ..
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet)
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Polymer Resources NY66-EX1 High Viscosity Nylon 66
Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as ..
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Flexural Modulus 3.28 GPa
476 ksi
ASTM D790
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Techmer ES HiFill® ABS GF10 A1 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast UF3 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast UF4 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast UF96 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flexural Modulus 3.28 GPa

@Temperature 93.0 °C
476 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Americas Styrenics MB3150 High Heat Crystal Polystyrene
Product CharacteristicsFast cycling due to high heat distortion temperatureHigh vicat softening temperatureExcellent clarity with slight blue tintGood toughnessFood Contact CompliantUL Classificatio..
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene
Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk ..
Copyright © lookpolymers.com All Rights Reserved