Arkema Group Nakan® RMA 705 N PVC, Rigid Injection Molding Grade

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Arkema
Trade Name Nakan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Nakan® RMA 705 N PVC, Rigid Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NAKAN RMA 705 N L is a rigid polyvinyl chloride compound developed for injection molding of various medium impact resistance applications.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 6.0 %
6.0 %
50 mm/min
Charpy Impact Unnotched NB
NB
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C
158 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.