Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Water Absorption 1.0 %

@Thickness 31.8 mm
1.0 %

@Thickness 1.25 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0070 cm/cm
0.0060 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9010 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 72.0 MPa
10400 psi
5.0 mm/min; ISO 527
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 4.41 GPa
640 ksi
ASTM D790
Izod Impact, Notched 0.720 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.35 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180
Descriptive Properties Value Comments
Filler / Reinforcement Glass Bead
Glass Fiber Reinforcement
Unspecified FillerReinfor., 35% Filler by Weight
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Regional Availability North America