Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.720 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.35 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GBF 1010 35 BLACK 13 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.720 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.35 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-10CF/15T Black Polycarbonate (PC) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | 0.5 in.; ASTM D256 |
Resirene Resirene® 4220 High Impact Polystyrene Features:High FlowEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityExternal LubricatedApplications:InjectionTV CabinetsTyping Machine CasesPrintersToysInformation provided by US distributor Cals.. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | 0.5 in.; ASTM D256 |
Resirene Resirene® 9720 High Impact Polystyrene Features:Medium FlowHigh Thermal ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingInjectionDisposablesGPPS/HIPS BlendsInformation provided by US distributor.. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
Plenco 50030 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
Plenco 50130 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Izod Impact, Notched | 0.720 J/cm @Temperature 0.000 °C |
1.35 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
Albis Plastics Polyamide 6/66 PA 152 GF30/02 BK8-1114 Black 30% Glass Fiber
(discontinued **) Semi-crystalline Nylon 6/66 (PA6/66)Characteristics: Industrial GradeApplications: Office Furniture, Gear, Housings and ConnectorsProcessing: Injection Molding (Melt Temperature: 465 -555°F, Mold .. |
|||
Izod Impact, Notched | 0.720 - 0.800 J/cm @Temperature -40.0 - -40.0 °C |
1.35 - 1.50 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.760 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Notched | 0.720 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.35 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Izod Impact, Notched | 0.720 J/cm @Temperature 23.0 °C |
1.35 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp GFL14 PSU LNP* Lubricomp* GFL14 is a compound based on Polysulfone containing Glass Fiber and PTFE Lubricant.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | |
UBE UBEPOL BR13HB HIPS (n-DM =0.03 wt %) Description: UBEPOL-BR13HB is characterized by its low solution viscosity compared with conventional grades and short dissolution time in styrene monomer. Its main merits are as follows:Short dissol.. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon D870 = Transparent Amorphous Nylon for Injection Molding, Unlubricated. D870L = Transparent Amorphous Nylon for Injection Molding, Lubricated.Data provided by the manufacturer |