Material Notes:
The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.5 %

@Thickness 3.18 mm
1.5 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.9 MPa
11300 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 75.8 MPa
11000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Yield 20 %
20 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded, Across Flow; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C

@Thickness 3.18 mm
149 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 60.0 - 107 °C
140 - 225 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Additive Heat Stabilizer
Appearance Black
Features General Purpose
Lubricated
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Extrusion
Extrusion Blow Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications