PolyOne Edgetek® PI-30GF/000 Polyether Imide (PEI)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PI-30GF/000 Polyether Imide (PEI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Water Absorption 0.18 %

@Thickness 3.18 mm
0.18 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 172 MPa
24900 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 - 5.0 %
4.0 - 5.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 221 MPa
32100 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.70 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C

@Thickness 3.18 mm
410 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 360 - 399 °C
680 - 750 °F
Descriptive Properties Value Comments
Features General Purpose
High Heat Resistance
Filler / Reinforcement Glass Fiber Reinforcement, 30% Filler by Weight
Forms Pellets
Generic Material PEI
Generic Name Polyether Imide (PEI)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
Uses Automotive Applications
Consumer Applications
General Purpose
Industrial Applications
Copyright © lookpolymers.com All Rights Reserved