Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 172 MPa | 24900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 604 35 HS Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PI-30GF/000 Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 172 MPa @Thickness 3.20 mm |
24900 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | ASTM D638 |
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI (Asia Pacific) LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | ASTM D638 |
Cheng Yu Plastic N6G30 Nylon 6, 30% Glass Filled |
|||
Tensile Strength, Yield | 172 - 241 MPa @Strain 0.200 % |
24900 - 35000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 172 - 379 MPa @Strain 0.200 % |
24900 - 55000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 172 - 379 MPa @Strain 0.200 % |
24900 - 55000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 172 - 379 MPa @Strain 0.200 % |
24900 - 55000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 172 MPa @Strain 0.200 %, Temperature 649 °C |
24900 psi @Strain 0.200 %, Temperature 1200 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Yield | 172 MPa | 24900 psi | |
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Tensile Strength, Yield | 172 MPa @Strain 0.200 % |
24900 psi @Strain 0.200 % |
|
ATI Allvac® 30, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |