A. Schulman POLYBATCH™ Ivory 9035 Concentrate Based In Polyethylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Ivory 9035 Concentrate Based In Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® 9035 is an ivory color concentrate containing based in polyethylene. This concentrate was designed to provide color and opacity in film and molding applications. POLYBATCH® 9035 contains heavy metal pigment(s) and is typically recommended for use at 5% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 56 %
56 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 45
pellets/gram