Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 124 MPa
18000 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 6.21 GPa
900 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256