Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GMF 600 A 40 HS Natural Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 % |
18000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-20GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF25 IM L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill FR® PA4/6 GF30 FR HS X 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant and Heat StabilizedUL File Number: E.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF20 L BK002 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Additive: LubricantFeatures: Lubricated and High FlowAppearance: BlackTPCI# 8376102Info.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M38 HS BK 38% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 38% Filler by Weight and Mineral Filler, 38% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabili.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF20 TL10 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: PTFE Lubricant (10%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PES GF20 TL15 LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightPTFE LubricantFeatures: Low Extractables and LubricatedInformation provided by TP Compos.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PPS GF/M65 BK 65% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 65% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill FR® PA4/6 GF30 FR HS X 30% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant and Heat StabilizedUL File Number: E.. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 % |
18000 psi @Strain 0.200 % |
|
Universal Wire Works 4043 (AMS 4190) Aluminum Alloy Filler Metal Alloy 4043 is a 5% silicon aluminum alloy designed to weld many similar and dissimilar cast and wrought aluminum parts. This alloy is excellent for types 4043, 6063, 5052, 6061, 355, 356 and others... |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
Vista Metals Duramold-5™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Clariant Renol 6608G33HSL Nylon 66, 33% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Tensile Strength, Yield | 124 - 172 MPa @Strain 0.200 % |
18000 - 25000 psi @Strain 0.200 % |
Annealed Sheet |
ATI Wah Chang Vanadium Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores.. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 124 MPa | 18000 psi | |
PCP-Canada Max 5® 5083 Cast Aluminum Mold Block Max 5® is characterized by an excellent dimensional stability. It is a 5083 alloy which provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materi.. |
|||
Tensile Strength, Yield | 124 - 185 MPa | 18000 - 26800 psi | Average value: 148 MPa Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |