Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.86 GPa | 850 ksi | Tangent; ASTM D790 |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Niche Polymer PPHG30BK Homopolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS (Asia Pacific) LNP* Thermocomp* AF004L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ecomass® 1080ZD94 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Techn.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ensinger Tecapeek® XP-90 Compression Molded PEEK Compound, 25% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | tangent; ASTM D790 |
Spartech EP6430 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |