Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen EP340G Sheet and Thermoforming Grade Polypropylene Moplen RP340G is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340G is a random copolymer particularly suitable for.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen EP340K Sheet and Thermoforming Grade Polypropylene Moplen RP340K is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340K is a random copolymer particularly suitable for.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen HP524J BDDP Film Grade Polypropylene Moplen HP524J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP524J is a homopolymer particularly suitable for BOPP (Tender) fil.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen HP600N Injection Molding Grade Polypropylene Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen RP370G Blow Molding Grade Polypropylene Moplen RP370G is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP370G is a copolymer particularly suitable for blow molding applicat.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
PolyMirae Moplen HP521M IPP/WQBF Grade Polypropylene Moplen HP521M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP521M is suitable for core resin of co-extrusion CPP film. Moplen .. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Hyosung Topilene B200 PP B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Hyosung Topilene B200P PP B200P Applications: Industrial pipesCharacteristics: Chemical resistanceInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Hyosung Topilene B201Y PP B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Hyosung Topilene F301U PP F301U Extrusion General HomopolymerApplications: Heavy duty bagCharacteristics:ProcessabilityWeatherabilityHigh tenacityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Hyosung Topilene F400 PP F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Hyosung Topilene F501 PP F501 Extrusion General HomopolymerApplications:Flat yarnRopeBandCharacteristics:ProcessabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 35.3 MPa @Thickness 3.20 mm |
5120 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 35.3 MPa @Thickness 3.20 mm |
5120 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical SH610S ABS, Excellent Surface, High Impact Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® 6331 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® 6431 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 35.3 MPa @Thickness 3.20 mm |
5120 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | 2 in/min; ASTM D638 |
ExxonMobil PP1024E4 Homopolymer Product Description: Medium melt flow rate homopolymer. Particularly suitable for general purpose injection moldingAvailability: North America Features:Autoclave SterilizableEthylene Oxide Steriliz.. |
|||
Tensile Strength, Yield | 35.3 MPa | 5120 psi | 2.0 in/min; ASTM D638 |
ExxonMobil Exxtral™ MDK340 Performance Polyolefin Product Description: A medium melt flow rate, 40% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc.. |