Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ISO 1183 |
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ISO 1183 |
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ISO 1183 |
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ISO 1183 |
Polimeri Europa Clearflex® H&T LGH 138 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 138 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, slip agent, antiblocking and processing aid, suitable for blown film extrusion.Films obtai.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ISO 1183 |
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | |
Teknor Apex TruVis Esters™ DIDA Di-IsoDecyl Adipate |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ASTM D1505/D792 |
Braskem Flexus® 9200 Blown Film Extrusion Polyethylene Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing .. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ASTM D1505/D792 |
Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Line.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ASTM D1505/D792 |
Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene Frozen chicken packages; Meat-based frozen packages.Additives: Antiblock, D, PPA, PEBDInformation provided by Braskem. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ASTM D1505/D792 |
Braskem LL118 Blown Film Extrusion Linear Low Density Polyethylene Description: LL218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and .. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ASTM D1505/D792 |
Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene Description: LL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties a.. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ASTM D1505/D792 |
Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene Liners, LDPE and HDPE blends; General use packages; Technical films for automatic packaging.Additives: Antiblock, DInformation provided by Braskem. |
|||
Specific Gravity | 0.917 g/cc | 0.917 g/cc | ISO 1183 |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |