Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL T 190 Styrene - Isoprene Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polimeri Europa Europrene® SOL T 190 Styrene - Isoprene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Europrene® SOL T 190 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 16% weight and diblock content is 25%. A non-staining, TNPP free antioxidant system is added during the production process.Key Features: Europrene® SOL T 190 is an easy processable, general purpose grade, characterized by an optimum balance of adhesive and cohesive properties.Main Applications: The polymer is designed for hot melt pressure-sensitive adhesive applications. Europrene® SOL T 190 is also used in bitumen modification when enhanced adhesive properties are required.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Brookfield Viscosity 0.10 cP
0.10 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow 9.0 g/10 min
<br>@Load 5.00 kg,<br> Temperature 190 °C
9.0 g/10 min
<br>@Load 11.0 lb,<br> Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM D412
Elongation at Break 1200 %
1200 %
ASTM D412
300% Modulus 0.00100 GPa
0.145 ksi
ASTM D412