3M 31U72C (Clear) Polyethylene Protective UV Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 31U72C (Clear) Polyethylene Protective UV Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Protective UV Tape 31U72C is a 3 mil clear polyethylene self-wound film coated with a medium-high tack adhesive system featuring UV resistance.Information provided by 3M
Physical Properties Metric English Comments
Thickness 83.8 microns
3.30 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D3759
Elongation at Break 450 %
450 %
ASTM D3759
Peel Strength 0.09861 kN/m
0.5625 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Clear