Plenco 6310 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6310 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.980 g/cc
0.0354 lb/in³
ASTM D1895
Density 1.86 g/cc
0.0672 lb/in³
ASTM D792
Water Absorption 0.082 %
0.082 %
ASTM D570
Linear Mold Shrinkage 0.0031 cm/cm
0.0031 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 80
80
ASTM D785
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 0.272 %
0.272 %
ASTM D638
Tensile Modulus 13.4 GPa
1940 ksi
ASTM D638
Flexural Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 11.5 GPa
1670 ksi
ASTM D790
Compressive Strength 162 MPa
23500 psi
ASTM D695
Izod Impact, Notched 0.163 J/cm
0.305 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.195 J/cm²
0.928 ft-lb/in²
ASTM D256
Impact 69
69
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C

@Temperature 40.0 - 130 °C
41.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 214 °C
417 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Shrinkage 0.156 %
0.156 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+13 ohm-cm
1.90e+13 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Dissipation Factor 0.0159
0.0159
ASTM D150
Arc Resistance 48 sec
48 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638