Polymer Property : Dielectric Strength = 310 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 12.2 - 40.0 kV/mm
310 - 1020 kV/in
Average value: 16.1 kV/mm Grade Count:34
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Plenco 4224 Phenolic, Granular, Transfer Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive ap..
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Plenco 7466 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plenco 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plenco 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plenco 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
IDI Composites 46-09 Thermoset Polyester, Molding
Abrasion resistant, electrical grade material with V-O flame resistance and moderate strength.Data provided by the manufacturer.
Dielectric Strength 12.2 kV/mm
310 kV/in
60Hz, Step-by-Step, wet; ASTM D149
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group..
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade
Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe..
Dielectric Strength 12.2 kV/mm

@Frequency 60.0 Hz
310 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided ..
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Plenco 2000 Phenolic, Granular, Compression Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Plenco 6310 Phenolic, Granular, Compression Molded
PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco.
Dielectric Strength 12.2 kV/mm

@Thickness 3.17 mm
310 kV/in

@Thickness 0.125 in
ASTM D149
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Devcon Wear Guard (High Temp) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Dielectric Strength 12.2 kV/mm
310 kV/in
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone
Low viscosity, white coating for motor windings to 1100°F (593°C)
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd
BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better ..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plenco 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties...
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo..
Dielectric Strength 12.2 kV/mm
310 kV/in
60 Hz, wet, SS; ASTM D149
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac
RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am..
Dielectric Strength 12.2 kV/mm
310 kV/in
ASTM D149
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock..