Mechanical Properties Metric English Comments
Tensile Modulus 13.4 GPa
1940 ksi
ASTM D638
Premix Premi-Glas® 3101-25 Polyester BMC
Premi-Glas® 3101-25 is a 25% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL ..
Tensile Modulus 13.4 GPa

@Temperature 23.0 °C
1940 ksi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Tensile Modulus 13.4 GPa

@Temperature 23.0 °C
1940 ksi

@Temperature 73.4 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Tensile Modulus 13.4 GPa
1940 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC
LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan..
Tensile Modulus 13.4 GPa

@Temperature 23.0 °C
1940 ksi

@Temperature 73.4 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Tensile Modulus 13.4 GPa
1940 ksi
ASTM D638
Plenco 6310 Phenolic, Granular, Compression Molded
PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco.
Tensile Modulus 13.4 GPa
1940 ksi
1mm/min; ISO 527
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Conditioned)
Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil..