Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Oxford Polymers 15GF-V0 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame Resistant
15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame ResistantInformation provided by Oxford Polymers.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Oxford Polymers PBT 15GF-V0 UL Listed Polybutylene Terephthalate (PBT)
UL Listed Polybutylene Terephthalate (PBT)Information provided by Oxford Polymers.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant
Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test..
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Annealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Ultem 1100EF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP WFI18 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WFI18 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Silicone.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C

@Thickness 6.40 mm
370 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics ULTEM HU1100 PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.
Deflection Temperature at 1.8 MPa (264 psi) >= 188 °C
>= 370 °F
ISO 75 Af
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic
Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s..
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Plenco 6310 Phenolic, Granular, Compression Molded
PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Adell BT-33 Nylon 6, 15% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East)