Plenco 4311 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4311 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized under component file E40654. 04311 is available in black or brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Water Absorption 0.29 %
0.29 %
ASTM D570
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 83
83
ASTM D785
Tensile Strength, Ultimate 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 0.58 %
0.58 %
ASTM D638
Tensile Modulus 8.80 GPa
1280 ksi
ASTM D638
Flexural Strength 78.0 MPa
11300 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Compressive Strength 186 MPa
27000 psi
ASTM D695
Izod Impact, Notched 0.174 J/cm
0.326 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.199 J/cm²
0.947 ft-lb/in²
ASTM D256
Impact 85
85
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 82.0 µm/m-°C

@Temperature 40.0 - 130 °C
45.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.500 W/m-K

@Temperature 100 °C
3.47 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 186 °C
367 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 27 %
27 %
ASTM D2863
Shrinkage 0.167 %
0.167 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.90e+12 ohm-cm
6.90e+12 ohm-cm
ASTM D247
Dielectric Constant 4.7
4.7
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
Short Time; ASTM D149
Dissipation Factor 0.037
0.037
ASTM D150
Arc Resistance 166 sec
166 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638