Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 82.0 µm/m-°C @Temperature 20.0 °C |
45.6 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
CTE, linear | 82.0 µm/m-°C @Temperature 40.0 - 130 °C |
45.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
CTE, linear | 82.0 µm/m-°C | 45.6 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
CTE, linear | 82.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Beijing Chemical Industry KAIFA® 201-G15R PBT Resin 20% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
CTE, linear | 82.0 µm/m-°C @Temperature 20.0 °C |
45.6 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |