Polymer Property : Flexural Modulus = 1330 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC
LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
Flexural Modulus 9.17 GPa
1330 ksi
ASTM D790
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Celanese VECTRA S540 LCP, 40% Mineral Reinforced  (Unverified Data**)
40% mineral filled grade, low warpage high flow.40% mineral filled grade, low warpage high flow.Information provided by Celanese
Flexural Modulus 9.20 GPa
1330 ksi
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
Flexural Modulus 9.17 GPa
1330 ksi
CW; ASTM D790
Haysite H1000 Polyester Laminate
Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide..
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ..
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This ..
Flexural Modulus 9.17 GPa
1330 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS
LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Flexural Modulus 9.14 GPa
1330 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2310EPR PEI
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Flexural Modulus 9.20 GPa
1330 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Flexural Modulus 9.18 GPa
1330 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ4860HR PBT
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Flexural Modulus 9.18 GPa
1330 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Flexural Modulus 9.20 GPa
1330 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear
LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
Flexural Modulus 9.14 GPa
1330 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF007 PA 6
LNP* THERMOCOMP* PF007 is a compound based on Nylon 6 resin containing 35% Glass Fiber.
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
Flexural Modulus 9.17 GPa
1330 ksi
ASTM D790
Teknor Apex Chemlon® 340G Nylon 610, Glass Fiber Reinforced
Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Polyplastics FR-PET® BN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178-93
Wellman EcoLon® MRGF1882-BK1(GPE) Nylon 66, 40% Mineral and Glass Reinforced
All information provided by Wellman Engineered Resins.
Flexural Modulus 9.20 GPa
1330 ksi
ASTM-D790
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber
A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristi..
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178-93
Wellman Wellamid® GF30-60 XE-NBK1 33% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178-93
Wellman Wellamid® GFX1624-BK(PTFE) 30% Glass Fiber Reinforced, Lubricated Nylon 66
Description: Glass Fiber Reinforced, Lubricated Nylon 66Information provided by Wellman.
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Plenco 4311 Phenolic, Granular, Compression Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Unitika A1025GO PA6, Flame Retardant, Dry
Information provided by Unitika Ltd.
Flexural Modulus 9.20 GPa
1330 ksi
cond; ISO 178
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Celanese Celstran® +PP-GF40-04CN15 PP, 40% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Adell WR-37 33% Glass Reinforced PET
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Celanese VECTRA S540 LCP, 40% Mineral Reinforced
40% mineral filled grade, low warpage high flow.Information provided by Celanese
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 125 Polypropylene, Glass Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790