Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 166 sec | 166 sec | ASTM D495 |
Plenco 4349 Phenolic, Granular, Injection Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Arc Resistance | 166 sec | 166 sec | ASTM D495 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |