Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 08235 Polyester BMC, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 08235 Polyester BMC, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable for a broad range of applications such as capacitor cans, electrical enclosures, etc. It is available in bulk or extruded form, natural and black. Other colors available upon request. It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Water Absorption 0.076 %
0.076 %
ASTM D570
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 45
45
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 0.52 %
0.52 %
ASTM D638
Tensile Modulus 13.9 GPa
2020 ksi
ASTM D638
Flexural Strength 112 MPa
16200 psi
ASTM D790
Flexural Modulus 12.6 GPa
1830 ksi
ASTM D790
Compressive Strength 132 MPa
19100 psi
ASTM D695
Izod Impact, Notched 3.60 J/cm
6.74 ft-lb/in
ASTM D256
Charpy Impact, Notched 3.60 J/cm²
17.1 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 223 °C
433 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.00078 %
0.00078 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.10e+15 ohm-cm
2.10e+15 ohm-cm
ASTM D247
Dielectric Constant 4.2
4.2
ASTM D150
Dielectric Strength 11.6 kV/mm
295 kV/in
Step by Step; ASTM D149
13.9 kV/mm
353 kV/in
Short Time; ASTM D149
Dielectric Breakdown 23000 V
23000 V
1hr 120C; ASTM D149
Dissipation Factor 0.0129
0.0129
ASTM D150
Arc Resistance 193 sec
193 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638
Users viewing this material also viewed the following: