Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.9 kV/mm | 353 kV/in | Short Time; ASTM D149 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Dielectric Strength | 13.9 kV/mm | 353 kV/in | Short Time; ASTM D149 |
Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Dielectric Strength | 13.9 kV/mm | 353 kV/in | Short Time; ASTM D149 |
Plenco 7321 Phenolic, Nodular, Compression Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |