Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
6.74 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Izod Impact, Notched | 3.60 J/cm | 6.74 ft-lb/in | ASTM D256 |
Nylene® Naxel™ AX190 PPE (Polyphenylene Ether) General Purpose Grade. Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 3.60 J/cm @Thickness 3.17 mm |
6.74 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade Superior impact strength, even at low temperature. Applications: helmets, shoe heels, bobbins, roller skates, bags, pipes, radiator grills, auto parts, appliance wheels. |
|||
Izod Impact, Notched | 3.60 J/cm | 6.74 ft-lb/in | ASTM D256 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Izod Impact, Notched | 3.60 J/cm | 6.74 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 3726 E ABS ExtrusionABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing.. |
|||
Izod Impact, Notched | 3.60 J/cm | 6.74 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 7626 ABS High ImpactABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processi.. |