Polymer Property : Flexural Modulus = 1830 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.6 GPa

@Temperature 23.0 °C
1830 ksi

@Temperature 73.4 °F
Conditioned; ISO 178
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Flexural Modulus 12.6 GPa

@Temperature 23.0 °C
1830 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Flexural Modulus 12.6 GPa
1830 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LCL33 is a compound based on Polyethereketone resin containg Carbon Fiber, PTFE. Added features include: Elecrtically Conductive , Internally Lubricated.
Flexural Modulus 12.6 GPa

@Temperature 23.0 °C
1830 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Flexural Modulus 12.6 GPa

@Temperature 23.0 °C
1830 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Flexural Modulus 12.6 GPa
1830 ksi
ISO 178
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Flexural Modulus 12.6 GPa
1830 ksi
ASTM D790
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc.
Flexural Modulus 12.6 GPa
1830 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon ZX05043 PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZX05043 is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE, Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 12.6 GPa
1830 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PX94085 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PX94085 is a compound based on PA6 resin, containing Glass Fiber.
Flexural Modulus 12.6 GPa
1830 ksi
ASTM D790
Plenco 08235 Polyester BMC, Compression Molded
PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable ..
Flexural Modulus 12.6 GPa
1830 ksi
ISO 178
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Copyright © lookpolymers.com All Rights Reserved