Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 00755 Melamine-Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 00755 Melamine-Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755 is available only in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.37 %
0.37 %
ASTM D570
Linear Mold Shrinkage 0.0076 cm/cm
0.0076 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 72
72
ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 0.87 %
0.87 %
ASTM D638
Tensile Modulus 10.3 GPa
1490 ksi
ASTM D638
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Compressive Strength 161 MPa
23400 psi
ASTM D695
Izod Impact, Notched 0.195 J/cm
0.365 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.206 J/cm²
0.980 ft-lb/in²
ASTM D256
Impact 120
120
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 178 °C
352 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 1.08 %
1.08 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+12 ohm-cm
1.40e+12 ohm-cm
ASTM D247
Dielectric Constant 7.2
7.2
ASTM D150
Dielectric Strength 4.80 kV/mm
122 kV/in
Step by Step; ASTM D149
7.50 kV/mm
191 kV/in
Short Time; ASTM D149
Dissipation Factor 0.080
0.080
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 525 V
525 V
ASTM D3638