Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Qualchem Danamid FES-23 HUV Polyamide 6 Impact resistant, cold. Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial light.Information provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Qualchem Danamid FES-23 Polyamide 6 Impact resistant, coldInformation provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 525 - 600 V | 525 - 600 V | Average value: 586 V Grade Count:61 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
LG Chemical RS-650 ABS, Extrusion, General Purpose Information Provided by LG Chem |
|||
Comparative Tracking Index | 525 V | 525 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Comparative Tracking Index | 525 V | 525 V | A solution |
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East.. |
|||
Comparative Tracking Index | 525 V | 525 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Comparative Tracking Index | 525 V | 525 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Comparative Tracking Index | 525 V | 525 V | A solution |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Comparative Tracking Index | 525 V | 525 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Comparative Tracking Index | 525 V | 525 V | Test solution A; IEC 60112 |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV2 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, flammability class V2, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning... |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Pocan® DP B 3235 XF 901510 PBT, 30% Glass Fiber
(discontinued **) PBT, 30% glass fibers, injection molding, improved flowability |