Compressive Strength 161 MPa

@Temperature 149 °C
23400 psi

@Temperature 300 °F
ASTM D695
Haysite H320 Polyester Composite
A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ..
Compressive Strength 161 MPa
23400 psi
ASTM D695
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Compressive Strength 161 MPa
23400 psi
ASTM D695
Plenco 1501 Polyester, Briquette, Transfer Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Compressive Strength 161 MPa
23400 psi
ASTM D695
Plenco 1508 Polyester, Briquette, Transfer Molded
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl..