Petromont 7001 Medium Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 7001 Medium Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusion equipment.Petromont HDPE 7001 is an unpigmented polyethylene compound which, after proper incorporation of carbon black, may be used for geomembrane applications, such as liners for landfills and surface impoundments, where polyethylene is the material of choice. Comprehensive information on such facilities is available in documents issued by the U.S.A EPA.
Physical Properties Metric English Comments
Density 0.9385 g/cc
0.03391 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 2000 hour
>= 2000 hour
F<sub>50</sub>; ASTM D1693-B
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
At 200°C with oxygen in aluminum pan.; ASTM D3895
Melt Flow 0.20 g/10 min
0.20 g/10 min
I<sub>2</sub>; ASTM D1238
20 g/10 min
20 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break >= 850 %
>= 850 %
ASTM D638
Flexural Modulus 0.650 GPa
94.3 ksi
ASTM D790
Descriptive Properties Value Comments
Process Sheet Extrusion
Users viewing this material also viewed the following: