Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9385 g/cc | 0.03391 lb/in³ | ASTM D1505 |
Petromont 7001 Medium Density Polyethylene Resin Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |