Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.20 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.20 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Characteristics: PPI Recommended Hydrostatic Design Bases (HDB): 1250.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9302 HDPE Yellow Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Applications:Natural Gas Distribution Piping and FittingsData provide.. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips HiD® 9647T HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat S.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
Melt Flow | 0.20 - 0.50 g/10 min | 0.20 - 0.50 g/10 min | |
Kazanorgsintez 102-17 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Melt Flow | 0.20 - 0.50 g/10 min | 0.20 - 0.50 g/10 min | |
Kazanorgsintez 102-21 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Melt Flow | 0.20 - 0.50 g/10 min | 0.20 - 0.50 g/10 min | |
Kazanorgsintez 153-15 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Melt Flow | 0.20 - 0.50 g/10 min | 0.20 - 0.50 g/10 min | |
Kazanorgsintez 153-23 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Melt Flow | 0.20 - 3.0 g/10 min | 0.20 - 3.0 g/10 min | on the basis of basic grades 10703-020, 10803-020, and 18503-020, for masterbatches of other applications (coloring general purpose products, coloring toys, coloring food containers |
Kazanorgsintez P2KP Polyethylene Pigment Masterbatches Production Method: P2KP polyethylene pigment masterbatches are produced on the basis of low density polyethylene with high content of masterbatches. Application: P2KP polyethylene pigment masterbatc.. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | @ 190 C/2160g; ASTM D1238 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Melt Flow | 0.20 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.20 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |
|||
Melt Flow | 0.20 g/10 min @Load 5.00 kg, Temperature 90.0 °C |
0.20 g/10 min @Load 11.0 lb, Temperature 194 °F |
ISO 1133/T |
Total HDPE XLS 12 B High Density Polyethylene - Pipes and Fittings HDPE XLS 12 B is a high performance hexene-based black compound, with a MRS 10 MPa - PE100 classification, primarily intended for extrusion of large diameter and thick wall pressure pipes.Key charac.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | ASTM D1238 |
Aclo Accutech ABS ABS834G30L Glass Reinforced |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | ASTM D1238 |
Aclo Accutech Polyethylene HD0232G20CV High Density Glass Reinforced Chemically Coupled Approved to GMP.PE.018 Black A12438 |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene HD Bottles Flakes High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 5.0 g/10 min | 0.20 - 5.0 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX 8000 VPL BLK Thermoplastic Elastomer TPV Product Information: BP Flex TPV's are partially vulcanized thermoplastic elastomers designed to meet higher end applications that require the following performance criteria.Product Features:Higher .. |
|||
Melt Flow | 0.20 - 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules Bottle Grade. Source: Italian post-consumer plastic bottles coming from collection of municipal waste and selected by PE/PP matrix. |
|||
Melt Flow | <= 0.20 g/10 min @Load 21.6 kg, Temperature 230 °C |
<= 0.20 g/10 min @Load 47.6 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 7001 Medium Density Polyethylene Resin Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis LE6022 Polyethylene Modified Jacketing Compound LE6022 is a black low density copolymer modified polyethylene compound. It is characterized by excellent crack resistance and mechanical properties and low temperature performance in combination wit.. |
|||
Melt Flow | 0.20 g/10 min | 0.20 g/10 min | I<sub>2</sub>; ASTM D1238/E |
Petromont 7002 Medium Density Polyethylene Resin Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HP3902 Pipe HDPE Natural Medium Density Hexene CopolymerApplications: Pipe for gas distribution, oilfield and other industrial pipe, telecommunications conduit.Formolene HP3902 is a high performance copolymer that i.. |