Polymer Property : Oxidative Induction Time (OIT) = 100 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
At 200°C with oxygen in aluminum pan.; ASTM D3895
Petromont 7000 Medium Density Polyethylene Resin
Petromont HDPE 7000 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is readily processed by blown sheet or flat die extrusi..
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
200°C
Ineos G36-10-150 HDPE
G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes...
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
at 200°C, black product - aluminum pan method
Ineos G36-24-150 HDPE
Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p..
Oxidative Induction Time (OIT) >= 100 min

@Temperature 200 °C
>= 100 min

@Temperature 392 °F
ASTM D3895
SCG Chemicals EL-Leneâ„¢ H511W High Density Polyethylene Wire & Cable Grade
Key Characteristics: Contains special metal deactivator, high mechanical properties, high speed extrusionRecommended Applications: Insulation of communication cablesInformation provided by SCG Che..
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
ASTM D3895
Chevron Phillips Marlex® 7104 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRGood melt strengthExcellent flexibilityGood processabilityGood glossHigh COFApplications: Landfill coversFlat and round-die productsCoext..
Oxidative Induction Time (OIT) >= 100 min

@Temperature 200 °C
>= 100 min

@Temperature 392 °F
ASTM D3895
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
This hexene copolymer is tailored for pipe applications that require:Good melt strengthGood pipe stiffnessOutstanding ESCRTypical corrugated pipe applications for HP076 include:Culverts and storm se..
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
At 200°C with oxygen in aluminum pan.; ASTM D3895
Petromont 7001 Medium Density Polyethylene Resin
Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi..
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
200°C with oxygen in aluminum pan; ASTM D3895
Petromont 7002 Medium Density Polyethylene Resin
Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi..