SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
Tensile Strength, Yield 3.04 MPa

@Strain 100 %
441 psi

@Strain 100 %
ASTM D412
5.59 MPa

@Strain 300 %
811 psi

@Strain 300 %
ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
Tear Strength 83.4 kN/m
476 pli
ASTM D624