Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
ND Industries SuperGlue Ethyl 300 General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II |
|||
Shear Strength | 17.2 MPa | 2500 psi | |
NextGen Adhesives G907-31 Epoxy Adhesive Description: NGAC G907-31 is a medium viscosity epoxy adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-31 provides excellent .. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives TURBO FUSE 2000CP FLUORESCENT Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE FLUORESCENT advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performan.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 110SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives TURBO FUSE SERIES 143 BLACK TOUGHENED (300 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The p.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 160SI Surface Insensitive (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives TURBO FUSE SERIES 170 LOW ODOR/LOW BLOOM (1500 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 170 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives TURBO FUSE SERIES 180 BLACK TOUGHENED (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The p.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 190 (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | |
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin Mix ratio 1 to 1 by weight.KONA 877 with HARDENER #112 is a versatile epoxy casting system developed for high performance production potting and encapsulating applications where low shrinkage and ra.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Al/Al, Tensile lap |
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an.. |
|||
Shear Strength | >= 17.2 MPa | >= 2500 psi | Al/Al, Tensile lap |
Master Bond EP21NDFG Two component epoxy compound for high performance applications Product Description: Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency.. |
|||
Shear Strength | >= 17.2 MPa | >= 2500 psi | Tensile, Al/Al |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
Shear Strength | >= 17.2 MPa | >= 2500 psi | Bond, Al to Al |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile lap, Al to Al |
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Aluminum, Initial |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Aluminum |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Green FRP, Cohesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Tensile Shear Adhesion, on a grit blasted steel |
3M Scotchkote™ RG 501 Urethane Metal Repair Scotchkote Urethane Metal Repair RG 501 has been specifically developed as a rapid curing repair system for rebuilding and repairing equipment requiring good mechanical strength.Product Features:Com.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, CRS/CRS tested after RT aging |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 17.2 MPa @Temperature 22.0 - 24.0 °C |
2500 psi @Temperature 71.6 - 75.2 °F |
Minimum MIL-A-8623 Type III Requirement |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Al, Hydraulic Oil at RT for 30 days |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Al, JP-4 for 30 days |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 17.2 MPa | 2500 psi | Overlap, Etched Al, JP-4 for 30 days |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 17.2 MPa @Temperature 24.0 °C |
2500 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 17.2 MPa @Temperature 21.0 °C |
2500 psi @Temperature 69.8 °F |
Overlap |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |