Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH &

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH &.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high tensile strength, high flexural modulus, low warpage, excellent dimensional stability, and low moisture absorption. This grade was designed specifically to be cost effective when high stiffness, good dimensional stability, and superior electrical properties are required. With a comparative tracking index of 450 volts and a deflection temperature of 505°F (263°C), this resin is a potential thermoset replacement in many electrical applications. Potential applications for AMODEL AF-1550 V0 resin include electrical relays, housings, motor starters, contactors, circuit breakers, and terminal blocks. This grade of AMODEL resin can also withstand the demanding vapor phase and infrared reflow soldering processes commonly used in the electronics industry for connectors and devices requiring surface mount technology.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.MatWeb has an entry for this material dry as molded.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Dry As Molded
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 116 MPa
16800 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 16.5 GPa
2390 ksi
ASTM D638
Flexural Yield Strength 177 MPa
25700 psi
ASTM D790
Flexural Modulus 14.1 GPa
2050 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 4.6

@Frequency 1e+6 Hz
4.6

@Frequency 1e+6 Hz
ASTM D150
4.7

@Frequency 100 Hz
4.7

@Frequency 100 Hz
ASTM D150
Dissipation Factor 0.018

@Frequency 100 Hz
0.018

@Frequency 100 Hz
ASTM D150
0.026

@Frequency 1e+6 Hz
0.026

@Frequency 1e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 321 - 338 °C
610 - 640 °F
Injection