Material Notes:
ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good resistance to heat (less than 230°C). The low level of internal stress reduces considerably the deformation during and after machining. Typical applications include automotive, structural foam molds, rubber molds, investment cast, low-pressure injection molds, R.T.M. and R.I.M. molding. It provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materials).Information provided by PCP-Canada.
Physical Properties Metric English Comments
Density 2.77 g/cc
0.100 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 81
81
Tensile Strength, Ultimate 262 MPa
38000 psi
Tensile Strength, Yield 138 MPa
20000 psi
Elongation at Break 7 %
7 %
in 2 inches
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 22.3 µm/m-°C

@Temperature 20.0 - 100 °C
12.4 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 162.5 W/m-K
1128 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 230 °C
446 °F
Component Elements Properties Metric English Comments
Aluminum, Al 92.38 - 94.56 %
92.38 - 94.56 %
as remainder
Chromium, Cr 0.050 - 0.25 %
0.050 - 0.25 %
Copper, Cu 2.7 - 3.25 %
2.7 - 3.25 %
Iron, Fe 0.85 - 1.15 %
0.85 - 1.15 %
Magnesium, Mg 0.95 - 1.25 %
0.95 - 1.25 %
Manganese, Mn <= 0.070 %
<= 0.070 %
Nickel, Ni 0.85 - 1.2 %
0.85 - 1.2 %
Silicon, Si <= 0.20 %
<= 0.20 %
Titanium, Ti 0.040 - 0.10 %
0.040 - 0.10 %
Zinc, Zn <= 0.15 %
<= 0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000044 ohm-cm
0.0000044 ohm-cm
Copyright © lookpolymers.com All Rights Reserved