Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000044 ohm-cm | 0.0000044 ohm-cm | |
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good .. |
|||
Electrical Resistivity | 0.0000044 ohm-cm | 0.0000044 ohm-cm | |
Vista Metals Duramold-2™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |