CTE, linear 22.3 µm/m-°C

@Temperature 20.0 - 100 °C
12.4 µin/in-°F

@Temperature 68.0 - 212 °F
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate
ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good ..
CTE, linear 22.3 µm/m-°C

@Temperature 20.0 - 100 °C
12.4 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..