Polymer Property : Thermal Conductivity = 1128 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 162.5 W/m-K
1128 BTU-in/hr-ft²-°F
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate
ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good ..