Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.77 g/cc | 0.100 lb/in³ | |
Pyrotek Pyrocast ZE Refractory Shapes Aggregate Base: MulliteApplicationsDoor lintel Breech plug Crucible bottoms Furnace rake Information provided by Pyrotek. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
Misumi ANP79 Aluminum Alloy Similar in hardness to 7075 Aluminum Alloy with lower internal stresses. Higher uniformity than 7075.Information provided by MISUMI Corporation. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
Ferro EG 3608 Metal Sealing Glass Type: Si-Ti Alkali Typical Powder Form: VSD Typical Application: Al Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals fo.. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
LATI Laticonther 47/1 CP/80 PP Copolymer High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Density | 2.77 g/cc @Temperature 25.0 °C |
0.100 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8436 Particularly resistant to sodium vapor and alkaline solutions, suitable to combinations with sapphire glass.Information provided by SCHOTT AG. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
Schott UG1 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
Superior Die Set FORTAL® HP Aluminum Alloy Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d.. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
Superior Die Set FORTAL® HR Aluminum Alloy Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d.. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good .. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | per Aluminum Association |
Alcoa 2324-T39 Aluminum Plate Alloy 2324-T39 is a higher strength version of alloy 2024-T351 and is a purity controlled composition variant of alloy 2024. It was developed for tension-dominated, fatigue and fracture critical pl.. |
|||
Density | 2.77 g/cc | 0.100 lb/in³ | |
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |