Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
ASTM D792
Filler Content 50 %
50 %
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 207 MPa
30000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 345 MPa
50000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Processing Properties Metric English Comments
Processing Temperature 271 - 288 °C
520 - 550 °F