Processing Properties Metric English Comments
Processing Temperature 271 - 288 °C
520 - 550 °F
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding
33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 271 - 288 °C
520 - 550 °F
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding
43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 271 - 288 °C
520 - 550 °F
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding
50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 271 °C
520 °F
Oxford Polymers PC 20 Unfilled Polycarbonate for Injection Molding
Unfilled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 271 - 327 °C
520 - 620 °F
Average value: 299 °C Grade Count:5
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..