Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.8 GPa | 2000 ksi | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Edgetek® SF-40GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester Vypet VNT 245 is a 45% fiberglass reinforced modified PBT / PET polyester injection molding compound designed for electrical and automotive applications requiring low warp and improved surface finis.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Techmer ES Statiblend® PPS GF40 EC BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightFeatures: Semi ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830L-50G Nylon 6, 50% Glass Reinforced Nylon 6, 50% glass reinforced resin.Data provided by the manufacturer |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | >= 13.8 GPa | >= 2000 ksi | |
Bulk Molding Compounds BMC 845 30% Glass Filled Vinyl Ester BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compressive creep at .. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | |
Bulk Molding Compounds BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled Description: BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compress.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and .. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric.. |
|||
Flexural Modulus | 13.8 - 15.2 GPa | 2000 - 2200 ksi | |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |